Inconel X750
2.4669, NiCr15Fe7TiAl, N07750, B 637 N07750 Type 1, B 637 N07750 Type 2, SB.637 N07750 Type 1, Inconel X750,
Inconel X750 Datasheet
Inconel X750 Superalloys: SAE AMS 5542N (2007) Chemical composition
C | Mn | Si | S | P | Cu | Fe | Co | Nb | Cr | Ni | Al | Ti |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤0.08 | ≤1.0 | ≤0.5 | ≤0.01 | ≤0.015 | ≤0.5 | 5.0-9.0 | ≤1.0 | 0.70-1.20 | 14.0-17.0 | 70- ≥ | 0.40-1.00 | 2.25-2.75 |
Inconel X750 Superalloys: SAE AMS 5542N (2007) specification
- SAE AMS 5542N (2007) - Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe Annealed
- SAE AMS 5582F (2012) - Nickel Alloy, Corrosion and Heat-Resistant, Seamless Tubing 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Solution Heat Treated, Precipitation Hardenable to 155 ksi (1069 MPa) Tensile Strength
- SAE AMS 5598E (2007) - Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 72Ni - 15.5Cr - 0.95 (Cb (Nb) + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode, Remelted or Vacuum Induction Melted, Solution Heat Treated, Precipitation-Hardenable
- SAE AMS 5667N (2015) - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Equalized, Precipitation Hardenable
- SAE AMS 5668J (2007) - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 7.0Fe - 2.5Ti - 1.0Cb (Nb) - 0.70Al 2100°F (1149°C) Solution and Precipitation Heat Treated
- SAE AMS 5669B (1965) - Alloy Bars, Corrosion and Heat Resistant Nickel Base - 15.5Cr - 0.95 (Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted
- SAE AMS 5670F (2005) - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe 1800°F (982°C) Solution Heat Treated, Precipitation-Hardenable
- SAE AMS 5671G (2007) - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800°F (982°C) Solution Heat Treated, Precipitation Hardenable
- SAE AMS 5698G (2007) - Nickel Alloy, Corrosion and Heat-Resistant, Wire 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe No. 1 Temper, Precipitation Hardenable
- SAE AMS 5699G (2007) - Nickel Alloy, Corrosion and Heat-Resistant, Wire 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Spring Temper, Precipitation Hardenable
- SAE AMS 5747D (2006) - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe Solution Heat Treated, Precipitation Hardenable
- SAE AMS 5779E (2003) - Alloy Welding Electrodes, Covered, Corrosion and Heat-Resistant 75Ni - 15Cr - 1.5 (Cb+Ta) - 1.9Ti - 0.55Al - 5.5Fe
- SAE AMS 5583E (2013) - Nickel Alloy, Corrosion and Heat-Resistant, Seamless Tubing 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Vacuum Melted Solution Heat Treated, Precipitation Hardenable to 170 ksi (1172 MPa) Tensile Strength
- SAE J 467b (1968) - Special Purpose Alloys ("Superalloys")
- SAE J 470 (1976) - Wrought nickel and nickel-related alloys
Inconel X750 Superalloys - mechanical properties
Heat treatment | Min | Max | Similar | Note |
---|
Heat treatment | Min | Max | Similar | Note |
---|
Heat treatment | Min | Max | Similar | Note |
---|
Heat treatment | Min | Max | Similar | Note |
---|
Heat treatment | Min | Max | Similar | Note |
---|
Heat treatment | Type | Min | Max | Similar | Note |
---|
Inconel X750 Superalloys delivers
- Bars, hot-rolled bars, hot-rolled round bars, cold-drawn round bars, hexagonal bars, octagonal bars, hot-rolled flat bars, cold-drawn flat bars, special-shaped steel
- Hot cold rolled strip and coils
- Hot Cold Rolled Plate Sheet
- Hot rolled and Cold drawn Shaped
- Hot rolled and cold drawn wire
- Forgings and forged bars