NICKEL 201
NICKEL 201,
NICKEL 201 Datasheet
NICKEL 201 Superalloys: UNS N02201 Chemical composition
C | S | Si | Cu | Ni | Fe |
---|---|---|---|---|---|
≤0.02 | ≤0.01 | ≤0.35 | ≤0.25 | Bal- ≥ | ≤0.4 |
NICKEL 201 Superalloys: UNS N02201 specification
- UNS N02201 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
- ASME Code Case 2249 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
- BS 3072 – 3074 (NA12) - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
- ASTM B 160 – B 163, B 366,B 725, B 730, B 751,B 775, B 829 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
- DIN 17740, 17750 – 17754 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
- ASME SB-160 – SB-163,SB-366, SB-725, SB-730,SB-751, SB-775, SB-829 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
- ISO 6207, 6208, 9723 – 9725 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
NICKEL 201 Superalloys - mechanical properties
Heat treatment | Min | Max | Similar | Note |
---|
Heat treatment | Min | Max | Similar | Note |
---|
Heat treatment | Min | Max | Similar | Note |
---|
Heat treatment | Min | Max | Similar | Note |
---|
Heat treatment | Min | Max | Similar | Note |
---|
Heat treatment | Type | Min | Max | Similar | Note |
---|
STANDARD PRODUCT FORMS
Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
PHYSICAL CONSTANTS AND THERMAL PROPERTIES
Density, Ib/in3........................................................................0.321
g/cm3......................................................................... 8.89
Melting Range, °F ...................................................2615 – 2635
°C ...................................................1435 – 1446
Specific Heat, Btu/lb•°F ....................................................0.109
J/kg•°C........................................................... 456
Curie Temperature, °F ........................................................... 680
°C ........................................................... 360
Permeability ........................................................ Ferromagnetic
Coefficient of Expansion, 70 – 200°F, 10-6 in/in •°F........ 7.3
21 – 93°C, µm/m• °C............ 13.1
Thermal Conductivity, Btu • in/ft2•h•°F ........................... 550
W/m• °C.......................................... 79.3
Electrical Resistivity, ohm• circ mil/ft..................................51
µΩ•m..............................................0.085
TYPICAL MECHANICAL PROPERTIES
(Annealed)
Tensile Strength, ksi.............................................................. 58.5
MPa............................................................ 403
Yield Strength (0.2% Offset), ksi...........................................15
MPa..................................... 103
Elongation, % ..............................................................................50
NICKEL 201 Superalloys delivers
- Bars, hot-rolled bars, hot-rolled round bars, cold-drawn round bars, hexagonal bars, octagonal bars, hot-rolled flat bars, cold-drawn flat bars, special-shaped steel
- Hot cold rolled strip and coils
- Hot Cold Rolled Plate Sheet
- Hot rolled and Cold drawn Shaped
- Hot rolled and cold drawn wire
- Forgings and forged bars